Specifications: 1.components:The paint is made of chlorinated rubber resin, plasticizer, modified resin , pigments, fillers and
solvents through modulation.
2.Characteristics: The paint is volatile coating and enjoys fast drying, good anti-corrosion, low construction
temperature, good resistance humid, corrosion resistance, chemical resistance and flame
retardance gas and salt spray resistant.
3.Functions: The paint is applicable to ships, bridges, port facilities, chemical equipment, iron and steel components
as surface preservative, as it is a high-performance anti-corrosion coating .
4.technical standards:
Projects standards
Exterior appearance of film smooth and meet the model requirements
Fineness no more than 25 um
Viscosity no more than 60s
Drying time (hard dry) 24 h
Adhesion no more than grade 2
Flexibility no more than 1mm
Hardness no more than 0.3
5.reference to construction
1.The paint enjoys short constrution cycle and can been sprayed,brushed and rool coated.
2.Thoroughly stir the paint and use exclusive chloride rubber thinner to dilute the viscosity.
3.The intervsl time of two paints should be more than 6 hours and maintain one week after finshing.
|